Product Details:
|
| Plate Type: | Double Layer Positive Thermal CTP Plate | Plate Thickness: | 0.15mm (0.20mm, 0.25mm, 0.30mm Available) |
|---|---|---|---|
| Sensitive Wavelength: | 830nm | Exposure Energy: | 110-130 Mj/cm2 |
| Aluminum Grade: | 1050/1060 H18 Aluminum Alloy | Run Length Unbaked: | 250,000-300,000 Copies (ordinary Ink) |
| Run Length Baked: | 500,000 Copies And Above | Resolution: | 1-99% At 200lpi, 240lpi At 10 Micron |
| Dot Reproduction: | Stable 1-99% Dot After 200,000 Impressions | Coating Color: | Blue |
| Max Plate Size: | 1650 X 1450mm | Application: | Newspaper Printing, Insert Printing, High Volume Commercial Work |
| Highlight: | Long Run Length CTP Plate,Double Layer Coating Plate,High Volume Web Press Plate |
||
Newspaper and insert work punishes a plate differently from commercial sheet-fed work: web tension, fast ink take-up and continuous roll changes. This 0.15mm double layer positive thermal CTP plate answers that with a two-stage coating - a solvent-resistant top layer over an adhesion layer - on a fine-grained 1050 H18 aluminum base. Actual run length depends on press condition, ink, paper and imaging content. 100 sheets per carton for 0.15mm, black photo protective paper interleaved, export cartons on fumigated pallets. MOQ 3000 square meters, 6 working days for stock formats, custom sizes in 15-25 days. Which platesetters does it run on? All mainstream 830nm thermal platesetters, no pre-heat required. Can you supply trial rolls or sample sheets? Yes, sample plates in your press format are available before the first order. Do you offer baked-grade plates for contract work? Yes, the same plate is bakeable for runs above 500,000 copies.0.15mm Double Layer Thermal CTP Plate for Long Run Newspaper Production
Designed around run length
Run length reference
Condition
Impression count
Typical job
Unbaked
250,000-300,000 copies
Daily newspaper, weekly inserts
Baked
500,000 copies and above
Long-run contract titles, catalogues
Specifications
Plate type
Double layer positive working thermal CTP plate
Thickness
0.15mm standard, other gauges on request
Max size
1650 x 1450mm, cut to press format
Sensitive wavelength
830nm
Resolution
1-99% at 200lpi, 240lpi at 10 micron
Processing
23 +/- 2 C, 25-30 seconds, standard positive thermal developer
Shelf life
18-24 months at 10-26 C, 40%-70% RH, flat storage, away from sunlight
Packing and delivery
FAQ
Contact Person: Jenny
Tel: +8615813828491